Grade  | PENSC-A  | |
Chemical structure  | %  | 99  | 
Other components  | 
  | no  | 
Density  | g/cm3  | >2  | 
Hardness  | HL  | 300  | 
Flexural Strength  | Mpa  | 35  | 
Coefficient of thermal expansion  | (10-6/K)  | -1~2.5  | 
Thermal conductivity at 20℃  | W/mk  | 75  | 
MAX-Temperature of use  | oxidizing  | 900℃  | 
vacuum  | 1800℃  | |
inert  | 2200℃  | |
RT Resistivity  | Ω.cm  | >1014  |